Lithium ions need usable paths as well as connected routes

More routes through an electrode can coexist with slower lithium movement when local energy differences trap ions. A peer-reviewed study combined atomic simulations with experiments on disordered lithium–manganese–titanium oxides. It found that balancing connectivity with site energies better describes transport. A partially ordered structure improved both properties, with laboratory capacity measurements supporting the approach for this material family.

Science··Evening
Coin cells clamped in test holders on a lab bench, beside an electrode disc coated in dark lithium–manganese–titanium oxide and a small vial of the same powder.

Additional routes can contain energetic traps

Lithium’s passage through a battery electrode depends on the energies it encounters along connected paths. In a peer-reviewed study of disordered rocksalt oxides, adding disorder improved the network of possible routes but widened differences between lithium sites. Ions could become trapped in favourable positions, slowing diffusion overall. Calculations and experiments focused on materials containing lithium, manganese, titanium and oxygen.[1]

Atomic models assess which connections are accessible

The researchers adapted three machine-learning models of atomic interactions and checked their energies, forces and stresses against quantum calculations. Lithium jumps between octahedral sites through a tetrahedral opening. Openings without adjoining transition-metal cations can offer easier passage. Counting their connections alone misses regions that energy differences make difficult to reach. A revised measure combined the geometry of the network with the accessibility of its sites.[1]

Structural rearrangement improves the laboratory result

One tested composition delivered 294 milliampere-hours per gram. In a separate structural comparison, a transition towards a partly disordered spinel-like state yielded 316 milliampere-hours per gram while improving connections and narrowing the spread of site energies. These capacities refer to electrode material. The calculations held the transition-metal skeleton fixed, describing the state before major rearrangement. Longer cycling can introduce metal migration, surface changes and particle damage beyond that model.[1]

References

  1. News sourceNature CommunicationsBattery electrode study weighs connected paths against energy traps↩1↩2↩3