Eigen RadarScience
Analysis

Interlocking joints shifted cracks in bridge beam tests

In tests of precast concrete bridge beams, a more strongly interlocking joint sent the main crack into the concrete itself. Researchers from institutions in China and Japan compared three shapes for the grooves where beam sections meet. The results helped them test a way of calculating how much bending those joints can withstand.

Science··Evening
Close-up detail of an interlocking joint and a bending crack running through the concrete in a precast bridge beam specimen after laboratory load testing.

Only the shape changed between beam tests

One peer-reviewed laboratory study asked what happens where sections of precast bridge beams meet. The team included researchers at Japan’s Tohoku University and China’s Tongji University and Liaoning Technical University. The researchers compared three groove shapes in joints filled with very high-strength concrete. They bent the specimens using the same loading procedure and kept the joint width and steel reinforcement arrangement fixed.[1]

The strongest interlock moved the main crack into concrete

The tests compared a rectangular groove, a diamond shape and a groove patterned on the Chinese character 干. The parts held together more strongly in the third configuration. There, the main crack ran through the concrete instead of following the boundary between the beam section and the joint. In the diamond-shaped specimen, cracks clustered around the projections of the joint. At peak load, the widest crack in the third specimen measured 1.65 millimetres. The maximum was 2.08 millimetres with the diamond and 2.36 with the rectangular groove.[1]

The force paths gave a way to estimate bending capacity

To estimate how much load a joint can take in bending, the team first mapped where the concrete is compressed and where the steel is pulled. It then used that map to calculate capacity. Compared with laboratory measurements and earlier test data, the estimate had a mean error of 11 percent. Full-size bridges and other joint designs remain outside the range tested.[1]

References