A thicker bolt shifted damage to the concrete in a bamboo wall-panel joint
In tests of joints for prefabricated bamboo and concrete wall panels, thicker glass-fiber bolts generally resisted more force. The gain narrowed at the largest diameter tested, where damage developed around the bolt's anchorage in the concrete. The experiments show where strengthening one part of the joint reached a limit in the tested design.
Science··Midday
The widest glass-fiber bolt held as its anchorage gave way
In a peer-reviewed Scientific Reports study, a team including China University of Geosciences in Beijing looked at the joint where an engineered bamboo layer passes force to the concrete in a prefabricated wall panel. In the tests, thinner glass-fiber-reinforced polymer bolts broke under forces that pushed the layers past each other. With the 18-millimeter bolt, the joint failed around the point where the bolt was anchored in concrete. The gains from increasing the diameter from 16 to 18 millimeters were smaller than for earlier increases.[1]
Bolts kept carrying load after the layers slipped further
Concrete, insulation and engineered bamboo made up the panel assembly. The team tested 13 joint specimens and tracked how far the concrete and bamboo moved relative to each other under successive loads. Epoxy restricted that movement early in the tests. Where adhesive was the sole connection, the load the joint could carry decreased sharply when the bond broke. Bolted joints continued to carry load after greater movement between the layers.[1]
The middle bolt spacing performed best in the tests
Along the length of the specimens, the researchers compared spacings from 100 to 200 millimeters. The 150-millimeter spacing gave the best overall results under the sideways loading used in the tests. Steel bolts were stiffer and withstood higher peak loads than their glass-fiber counterparts. The laboratory series focused on joints and left the long-term behavior of full-sized walls outside its scope.[1]