A concrete mix with waste glass and sisal proved stronger in tests
In a single laboratory study, a concrete mix containing waste glass powder and sisal plant fibres outperformed plain concrete in three strength tests after 28 days. The researchers compared 25 mixtures and also trained models to predict strength. Those predictions became less accurate when the team tested them on formulations held entirely out of training.
Science··Morning
One mix led the tests in compression, splitting and bending
Researchers at India’s KPR Institute of Engineering and Technology and partner institutions tested concrete in a peer-reviewed laboratory study, keeping the ratio of water to binder the same while varying the amount of waste glass powder and sisal fibre. The leading mix reached 33 MPa in compression, 4.8 MPa in splitting tension and 6.1 MPa in bending. Several nearby mixes gave similar results in compression and bending.[1]
Repeated specimens mostly came from the same batch
The experiment used 750 specimens, with 10 for every combination of mix and test. Most of these groups came from a single batch, so the results show how much samples within a batch varied. Separate batches remain to be compared. In the splitting test, the joint effect of glass and fibre exceeded the sum of their individual contributions. The authors discuss fibres bridging cracks as a possible explanation.[1]
Predictions worsened for unfamiliar mixes
The researchers trained models using their own measurements, published tests and synthetic examples generated from measured values. The models performed better when specimens from a given formulation could appear in training and testing. Their estimates were less accurate when whole mixes were kept out of training and the synthetic examples were rebuilt from the remaining data. The team also tested results from other laboratories, but had only 16 such records.[1]