Plastic with lighter lignin stretched further before breaking in lab tests
A US laboratory study at the State University of New York found that lighter molecules from lignin, a component of wood, spread more evenly through a molten plastic. At the same filler loading, the blend stretched further before it broke than a blend made with unseparated lignin. The result comes from a peer-reviewed experiment on lab specimens.
Science··Evening
AI image
Lighter lignin formed fewer clumps in the melt
US researchers at the State University of New York, including Nara Han, tested whether lignin, a component of wood, would mix into a type of polyester as a filler. In the peer-reviewed experiment, the blend with the lightest portion of lignin showed fewer clumps under the microscope than the blend with the original lignin. The team had first sorted the lignin into fractions using mixtures of ethanol and water.[1]
Samples stretched by different amounts at the same loading
When lignin made up 1 percent of the blend by weight, the samples with the lightest fraction stretched by 1,187 percent before breaking. Samples made with the unsorted lignin reached 877 percent at the same loading. The lightest fraction’s blend had a lower tensile strength than the plastic without filler. Samples made without lignin stretched by 1,105 percent before breaking.[1]
A higher filler share changed the result
At a light lignin content of 5 percent, the specimens stretched by 1,043 percent at the point of rupture. At that concentration the blend also showed higher absorption of ultraviolet light and lower permeability to water vapour. The findings come from a single study of samples made in the lab. The researchers compared the blends using moulded specimens. The experiment leaves industrial production performance and the cost of separating the lignin open.[1]