The first layer steers the crystal

A team from Delft University of Technology’s QuTech center and the Netherlands Organisation for Applied Scientific Research changed the starting surface for growing tantalum on sapphire. In laboratory work awaiting peer review, the researchers laid down titanium first. The control film grew mostly as beta tantalum. Titanium equivalent to half an atomic layer left both crystal phases present. At roughly one atomic layer, X-ray diffraction showed the alpha phase alone. The interface between the materials became a point of control at the first step of fabrication.[1]

For fabrication, the most valuable result is that two deposition systems working under different conditions yielded the same crystal phase. The thickness range that produced pure alpha tantalum ended sooner in one system than in the other. To reproduce the result, another lab needs to map titanium thickness against crystal structure on its own machine. The authors suggest the titanium may relieve stress at the interface. The machine-dependent thickness limit suggests that details of how that interface forms could also matter.[1]

From film to circuit

A resonator holds microwave energy for a time. How quickly the energy dissipates tests what the coating can do in a circuit. The Delft team compared devices of similar geometry. The optimized titanium-seeded film performed on a par with the conventional high-temperature route. Geometry matters for that comparison. Two resonators cut from the same film can show different losses when different amounts of electric field reach their surfaces. Matching the shapes helps isolate the contribution of the film.[1]

The coating also worked in a test circuit of 10 superconducting qubits. The team measured an average energy relaxation time of 96 ± 19 microseconds. That is a direct check that the film can go through the circuit fabrication steps. The resonators exposed a separate issue. Films subjected to prolonged oxide removal and a sample grown at high temperature showed an extra loss as the devices warmed. The researchers considered the motion of magnetic flux vortices as one possible explanation. Changes at the surface after oxide removal could also contribute. Measurements that vary the magnetic field under controlled conditions could help distinguish the contributions.[1]